Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 6375N Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 6375N Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Copolymer For High Speed Injection Molded Applications Formolene® 6375N is a very high melt flow, low impact copolymer of polypropylene. It is designed for such applications as packaging, housewares, and consumer goods and generally lighter weight components. It is characterized by easy mold flow, excellent physical property balance and finished product dimensional stability. Formolene® 6375N meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 75 g/10 min

@Temperature 230 °C
75 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4200 psi
2" (50mm) per min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.641 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648