Formosa Plastics Formolene® 5181K Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 5181K Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer for Extrusion Applications Including Straws Formolene® 5181K is a high molecular weight, highly isotactic, polypropylene homopolymer containing anti-stat designed for straws and cutlery. It contains a unique combination of stabilizers, which give it process stability and good end use performance. Formolene® 5181K meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min

@Temperature 230 °C
5.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 35.2 MPa
5100 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 23.0 °C
0.700 ft-lb/in

@Temperature 73.4 °F
ASTM D256