Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 5144H Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 5144H Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer for Appliance Applications Formolene® 5144H is a highly isotactic polypropylene homopolymer designed for consumer products and appliance applications requiring long-term heat-aging resistance and flexural endurance. 5144H has earned a UL continuous service rating of 65°C with recognition for typical use in laundry equipment.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Temperature 230 °C
2.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 10 %
10 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648