Formosa Plastics Formolene® 5143S Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 5143S Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143S is a higher melt flow homopolymer designed for light weighting of components. Its very high stiffness enables reduction of side walls and component weights without loss of top loading strength. It permits faster cycle times both in the extrusion and forming phases which can result in better process efficiencies. It is an excellent choice for ‘see-through’ house wares and rigid packaging. Formolene® 5143S has been formulated without components containing animal derivatives. Formolene® 5143S meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.0 g/10 min

@Temperature 230 °C
3.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.00 MPa
580 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648