Formosa Plastics Formolene® 5140N Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 5140N Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer for Injection Molded Applications Formolene 5140N is a highly isotactic, polypropylene homopolymer with fast cycle time and improved mold release. It has use in injection molded applications including closures and thin wall container programs. It contains a unique combination of stabilizers and additives, including elevated levels of antistat which provides excellent processability and good end use performance. Formolene 5140N meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Temperature 230 °C
12 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa
5100 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: