Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Random Copolymer for Extrusion and Thermoforming Applications Formolene® 3302B is a low melt flow random with excellent clarity, fast cycle time and easy mold release, designed for extrusion processing and thermoforming. It contains a unique combination of stabilizers and additives, which provides excellent processability and good end use performance. Formolene® 3302B meets all requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.3 g/10 min

@Temperature 230 °C
2.3 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4200 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 13 %
13 %
2" (50mm) per min; ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 2.67 J/cm

@Temperature 23.0 °C
5.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Optical Properties Metric English Comments
Haze 12 %
12 %
Plaque; FPC method
Copyright © lookpolymers.com All Rights Reserved