Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Melt Flow | 10 g/10 min @Temperature 230 °C |
10 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 90 | 90 | ASTM D785 |
Tensile Strength, Yield | 16.5 MPa | 2400 psi | 2" (50mm) per min.; ASTM D638 |
Elongation at Yield | 7.0 % | 7.0 % | 2" (50mm) per min.; ASTM D638 |
Flexural Modulus | 0.731 GPa | 106 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Izod Impact, Notched | NB | NB | ASTM D256 |
7.05 J/cm @Temperature -18.0 °C |
13.2 ft-lb/in @Temperature -0.400 °F |
ASTM D256 | |
Impact | 57 | 57 | ft-lb/in Notched Charpy @23°C/73°F; ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.0 °C | 169 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 47.0 °C | 117 °F | ASTM D648 |