Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 2610A Compounding and Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 2610A Compounding and Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact CopolymerApplications: Automotive compounds, lawn and garden products, and appliances.Formolene 2610A is a high impact copolymer of polypropylene designed for such applications as automotive compounds and injection molding of lawn and garden products and appliances. It is characterized by its easy mold flow, excellent physical property balance of stiffness and impact at room temperature and sub ambient conditions as well as finished product dimensional stability. It contains a unique combination of stabilizers which give it excellent processing and usage performance.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min

@Temperature 230 °C
10 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 20.3 MPa
2950 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 6.0 %
6.0 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
0.908 J/cm

@Temperature -30.0 °C
1.70 ft-lb/in

@Temperature -22.0 °F
ASTM D256
1.01 J/cm

@Temperature -18.0 °C
1.90 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648