Material Notes:
Improved compressive strength and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
ASTM 1457-62 T
Deformation 5.0 %
5.0 %
14 MPa, 100 h, 23°C; ASTM D621-59
Mechanical Properties Metric English Comments
Ball Indentation Hardness 40.0 MPa
5800 psi
ASTM 1457-62 T
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM 1457-62 T
Elongation at Break >= 100 %
>= 100 %
ASTM 1457-62 T
Coefficient of Friction, Dynamic 0.16 - 0.19
0.16 - 0.19
v = 1 m/s
0.18 - 0.20
0.18 - 0.20
v = 1.9 m/s
Abrasion 0.20
0.20
mm of depth after 200 hrs load duration; Partner Material ST 50
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 100 °C
38.9 µin/in-°F

@Temperature 212 °F
DIN 52328
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
DIN 53482
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
DIN 53482