Material Notes:
FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume metal powder and 40% volume plastic. The mixture (referred to as feedstock) is then injection molded at relatively low temperatures and pressures in conventional plastic injection molding machines. The molded green parts are then thermally processed in two steps. First, the binder is removed by evaporation in an operation called debinding. Next, the part is sintered in a dry hydrogen atmosphere, which densifies the part isotropically. The complex shape of the original molded part is retained throughout the process, and close tolerances can be achieved. Density is typically 95-98% of the wrought metal; mechanical properties and corrosion resistance are similar to wrought materialInformation provided by FloMet LLC.
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65
65
Tensile Strength, Ultimate 379 MPa
55000 psi
Tensile Strength, Yield 241 MPa

@Strain 0.200 %
35000 psi

@Strain 0.200 %
Elongation at Break 25 %
25 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 17 %
17 %
Iron, Fe 83 %
83 %
As remainder
Electrical Properties Metric English Comments
Magnetic Permeability <= 2000
<= 2000
µ<sub>max</sub> in G/Oe with a magnetizing field of 25 Oe.
Magnetic Coercive Force, Hc 1.2 Oe
1.2 Oe
Magnetic Saturation Flux Density, Bmax 11900 Gauss
11900 Gauss
Magnetizing field of 25 Oe.
16200 Gauss
16200 Gauss
Magnetizing field of 500 Oe.
Magnetic Remanence, Br 5300 Gauss
5300 Gauss
Magnetizing field of 25 Oe.