Material Notes:
Random copolymer, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: Radiation resistant and good contact clarity.Applications: Injection molding: radiation sterilizable medical devices and lab ware.FDA Notes: 21 CFR 177.1520 (c)3.1Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Modulus of Elasticity 1.105 GPa
160.3 ksi
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
23° C; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648