Flint Hills P9G8Z-036 Polypropylene Specialty Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P9G8Z-036 Polypropylene Specialty Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Broad MWD Homopolymer. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion coatingInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 72 g/10 min
72 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 1250 MPa
181000 psi
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 2.00 J

@Temperature 23.0 °C
1.48 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 1320 MPa
191000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ASTM D648