Material Notes:
Features: Good impact/stiffness balance. Product does not contain animal derived components.Applications: Injection Molding - appliance components, consumer durables, caps and closures.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.186 GPa
172.0 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Gardner Impact 24.0 J

@Temperature -30.0 °C
17.7 ft-lb

@Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1