Flint Hills P6G2N-095 Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P6G2N-095 Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent stiffness and impact resistance, nucleated, suitable for retort and hot fill applications. Product does not contain animal derived components.Applications: Blow molding, sheet/thermoforming for food, personal care, household chemicals and industrial parts.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
Tangent, 1.3 mm/min; ASTM D790
Izod Impact, Notched 6.03 J/cm
11.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
234 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.2a