Material Notes:
Impact copolymer, UL certified.Features: LTHA, controlled rheology, and extra high impact strength.Applications: Injection molding: automotive, toys, and containers.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 0.670 GPa
97.2 ksi
Tangent; ASTM D790
Gardner Impact >= 36.0 J

@Temperature -30.0 °C
>= 26.6 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648