Material Notes:
Features: Radiation resistant. Product does not contain animal derived components. Phthalate-freeApplications: Injection molded parts. Radiation sterilizable medical devices and lab wareInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 27 g/10 min
27 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Modulus 0.759 GPa
110 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a
USP Class VI certified