Flint Hills P5G2N-093 Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5G2N-093 Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Nucleated. Product does not contain animal derived components.Applications: Compression molding, Caps and ClosuresInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.2 MPa
4530 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.215 GPa
176.2 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 1140 MPa
165000 psi
ASTM D790
Izod Impact, Notched 2.18 J/cm
4.08 ft-lb/in
ASTM D256
Gardner Impact >= 36.2 J
>= 26.7 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.2a