Flint Hills P5C6Z-075 Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5C6Z-075 Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Phthalate-free.Applications: Fibers, BCF, SpunbondedInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 38 g/10 min
38 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.096 GPa
159.0 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 1027 MPa
149000 psi
ASTM D790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.2a