Flint Hills P4G4K-205 Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P4G4K-205 Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Clarified material. Product does not contain animal derived components. Phthalate-free.Applications: Cast FilmInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.81 GPa
263 ksi
ASTM D790
Flexural Modulus, 1% Secant 1740 MPa
252000 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Gardner Impact 1.40 J
1.03 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C
243 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 1.1a