Material Notes:
Homopolymer, FDA compliantFeatures: Antistat.Applications: Extrusion: straw grade.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 4.2 g/10 min
4.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.36 GPa
197 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
23° C; ASTM D256
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648