Material Notes:
Features: Nucleated and Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Closures and cutleryInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 3358 MPa
487000 psi
ASTM D790
Izod Impact, Notched 0.300 J/cm

@Temperature 23.0 °C
0.562 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact <= 0.904 J

@Temperature 23.0 °C
<= 0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 3257 MPa
472400 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648