Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills AP7310-HS Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills AP7310-HS Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultra high impact copolymer, UL certified, and FDA compliant.Features: Heat stabilized.Applications: Injection molding: appliance components, automotive exterior and underbody components, construction (housing components), equipment housings, and tool boxes.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
Tangent; ASTM D790
Gardner Impact >= 35.0 J

@Temperature -30.0 °C
>= 25.8 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Users viewing this material also viewed the following: