Flint Hills 21N2A Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Blow Molding Grade
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills 21N2A Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: FDA Compliant, High Flexural Modulus and High Heat Deflection TemperatureApplications: Thermoforming, Extrusion, Blow MoldingInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 2.3 g/10 min
2.3 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 40.3 MPa
5850 psi
ASTM D638
Elongation at Yield 4.6 %
4.6 %
ASTM D638
Flexural Modulus 2.25 GPa
326 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 2120 MPa
307000 psi
ASTM D790
Izod Impact, Notched 0.215 J/cm
0.403 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 1.1a