Material Notes:
Features: Excellent clarity, blush resistant and good flexural modulus. Product does not contain animal derived components.Applications: Injection Molded - Lab ware, food packaging and medical. Suitable for autoclave sterilization processes in the presences of aqueous solutions.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 977 MPa
142000 psi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D648
Optical Properties Metric English Comments
Haze 3.7 %

@Thickness 0.635 mm
3.7 %

@Thickness 0.0250 in
ASTM D1003
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a
USP Class VI certified