Fine Organics FINALUX GCC 10 Composite Lubricant

Category Fluid , Lubricant , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Fine Organics
Trade Name FINALUX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fine Organics FINALUX GCC 10 Composite Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: One pack lubricant specially suggested for PVC cable compound used for insulating/sheathing purpose (high filler levels).Information provided by Fine Organics
Physical Properties Metric English Comments
Additive Loading 1.0 - 2.5 %
1.0 - 2.5 %
P PVC
Thermal Properties Metric English Comments
Melting Point 95.0 - 105 °C
203 - 221 °F
Descriptive Properties Value Comments
Influence on Transparency Opaque
Lubricating Effect Internal/External
Physical Form Solid