Material Notes:
Applications: Lubricant of higher compatibility for rigid PVC films, fittings, profiles and other Sn-mercaptide stabilized articles, flow improver and internal, mold release agent for SBC/SAN/EVA, slip agent for ABS.Information provided by Fine Organics
Physical Properties Metric English Comments
Additive Loading 0.50 - 2.0 %
0.50 - 2.0 %
R PVC
Thermal Properties Metric English Comments
Melting Point 65.0 - 75.0 °C
149 - 167 °F
Descriptive Properties Value Comments
Influence on Transparency Clear
Lubricating Effect Internal
Physical Form Solid
Users viewing this material also viewed the following: