Fiberfil® M-2450 BK9083 Polypropylene Copolymer, 20% Talc

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer FiberFil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® M-2450 BK9083 Polypropylene Copolymer, 20% Talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Melt Flow 1.0 g/10 min
1.0 g/10 min
less than, 230/2.16 (typical); ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527
Elongation at Yield 80 %
80 %
ISO 527
Tensile Modulus 2.100 GPa
304.6 ksi
ISO 527
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Izod Impact, Notched (ISO) 26.5 kJ/m²
12.6 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-2