Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer FiberFil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0030 in/in

@Thickness 0.125 in
ASTM D955
0.0030 - 0.0040 cm/cm

@Thickness 6.35 mm
0.0030 - 0.0040 in/in

@Thickness 0.250 in
ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
230/2.16 (typical); ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Flexural Strength 56.0 MPa
8120 psi
ASTM D790
Flexural Modulus 2.65 GPa
384 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
276 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648