Material Notes:
Antishock rolling shutters
Physical Properties Metric English Comments
Density 1.42 - 1.46 g/cc
0.0513 - 0.0527 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ISO R 527
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO R527
Elongation at Break 130 %
130 %
ISO R 527
Izod Impact, Unnotched 8.80 - 9.20 J/cm

@Temperature 23.0 °C
16.5 - 17.2 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306