Material Notes:
Sheath PVC/PU for low temperatures
Physical Properties Metric English Comments
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77
73 - 77
ISO R 868
Tensile Strength at Break 15.0 MPa
2180 psi
ISO R 527
Elongation at Break 310 %
310 %
ISO R 527
Abrasion 90
90
[mm³]; DIN 53516
Thermal Properties Metric English Comments
Brittleness Temperature -36.0 °C
-32.8 °F
Cold Flex; ISO 458/2