Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Transparent
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Profiles, UL Class V2
Physical Properties Metric English Comments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 62 - 66
62 - 66
ISO R 868
Tensile Strength at Break 13.0 MPa
1890 psi
ISO R 527
Elongation at Break 360 %
360 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Flammability, UL94 V-2
V-2
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified