Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anti-impact connectors and components
Physical Properties Metric English Comments
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO R 527
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO R 527
Elongation at Break 140 %
140 %
ISO R 527
Thermal Properties Metric English Comments
Vicat Softening Point 58.0 - 60.0 °C
136 - 140 °F
ISO R 306
Descriptive Properties Value Comments
Properties according to Pharmacopoeia 4th edition OK