Fainplast Compounds MPH 62/H Medical Flexible PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds MPH 62/H Medical Flexible PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Technical tubes and peristaltic pump segments no DOP
Physical Properties Metric English Comments
Density 1.17 - 1.21 g/cc
0.0423 - 0.0437 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 64
60 - 64
ISO R 868
Tensile Strength at Break 12.0 MPa
1740 psi
ISO R 527
Elongation at Break 410 %
410 %
ISO R 527
Descriptive Properties Value Comments
Properties according to Pharmacopoeia 4th edition NO