Fainplast Compounds HGKA 0183 Flexible PVC, Sheathing for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HGKA 0183 Flexible PVC, Sheathing for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheathing high LOI
Physical Properties Metric English Comments
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 15.0 MPa
>= 2180 psi
ISO R 527
Elongation at Break >= 200 %
>= 200 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 40 %
40 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 130
CEI 20-34/3-2