Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds GK 89/2 Flexible PVC, Flame Retardant Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GK 89/2 Flexible PVC, Flame Retardant Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Special cables
Physical Properties Metric English Comments
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 280 %
>= 280 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -23.0 °C
-9.40 °F
Cold Flex; ISO 458/2
Oxygen Index 40 %
40 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 50
CEI 20-34/3-2