Fainplast Compounds GK 86/R Flexible PVC, Flame Retardant Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GK 86/R Flexible PVC, Flame Retardant Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrocarbon resistant
Physical Properties Metric English Comments
Density 1.42 - 1.46 g/cc
0.0513 - 0.0527 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 87
83 - 87
ISO R 868
Tensile Strength at Break >= 17.0 MPa
>= 2470 psi
ISO R 527
Elongation at Break >= 320 %
>= 320 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 26 %
26 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 45
CEI 20-34/3-2