Fainplast Compounds CTS 75 Flexible PVC, Extrusion Modified with Rubber

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds CTS 75 Flexible PVC, Extrusion Modified with Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gas pipe covering
Physical Properties Metric English Comments
Density 1.28 - 1.32 g/cc
0.0462 - 0.0477 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77
73 - 77
ISO R 868
Tensile Strength at Break 18.0 MPa
2610 psi
ISO R 527
Elongation at Break 250 %
250 %
ISO R 527