Fainplast Compounds CRKA 87 Flexible PVC, Flame Retardant Electrical Bedding Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds CRKA 87 Flexible PVC, Flame Retardant Electrical Bedding Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant bedding
Physical Properties Metric English Comments
Density 1.80 - 1.84 g/cc
0.0650 - 0.0665 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 90
86 - 90
ISO R 868
Tensile Strength at Break >= 6.00 MPa
>= 870 psi
ISO R 527
Elongation at Break >= 100 %
>= 100 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 35 %
35 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 35
CEI 20-34/3-2