Material Notes:
Product Description: Vistalon 878P rubber is a medium Mooney, medium ethylene copolymer with a narrow molecular weight distribution. It is applicable for use in modification of plastics, including the production of TPOs. This product is sold in pellet form.Key Features: Easy processing and mixing.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Mooney Viscosity 52

@Temperature 125 °C
52

@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
Descriptive Properties Value Comments
Ethylene Content 60.0 wt%
ASTM D3900
Users viewing this material also viewed the following: