ExxonMobil Vistalon™ 8600 Bimodal EPDM Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Vistalon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistalon™ 8600 Bimodal EPDM Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vistalon 8600 EPDM rubber is a grade of high molecular weight with a low ethylene content and a high diene level. It is produced with ExxonMobil Chemical's proprietary technology offering bimodal molecular weight distribution (MWD). This grade is ideal for the manufacture of sponge profiles combining a high collapse resistance and smooth extrusion.Key Features:Designed for: Constant quality of mixed compound.Improved productivity of mixing and sponge extrusion.Reduced inventories by using a single grade.High collapse resistance. Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Mooney Viscosity 81

@Temperature 125 °C
81

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
ENB Content 8.9%
ASMT D6047
Ethylene Content 58%
ASTM D3900