Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Vistalon™ 7500 Bimodal EPDM Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Vistalon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistalon™ 7500 Bimodal EPDM Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vistalon 7500 EPDM rubber is a grade of high molecular weight with a low ethylene content and a high diene level. It is produced with ExxonMobil Chemical's proprietary technology offering bimodal molecular weight distribution (MWD). This grade is ideal for the manufacturing of profiles and hoses combining high collapse resistance and smooth extrusion.Key Features: Consistent quality of mixed compound.Improved productivity of mixing, extrusion and molding.Reduced inventories by using a single grade.High collapse resistance.High elasticity with easy processing.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Mooney Viscosity 82

@Temperature 125 °C
82

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
ENB Content 5.7%
ASMT D6047
Ethylene Content 56%
ASTM D3900
Users viewing this material also viewed the following: