Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Varsol™ 140 Non-dearomatized Fluid

Category Fluid
Manufacturer Exxon Chemical
Trade Name Varsol™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Varsol™ 140 Non-dearomatized Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.850 g/cc

@Temperature 15.0 °C
0.0307 lb/in³

@Temperature 59.0 °F
ISO 12185
Vapor Pressure <= 0.000133 bar

@Temperature 20.0 °C
<= 0.100 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 280 °C
536 °F
Initial; ASTM D86
Flash Point 139 °C
282 °F
Method A; ASTM D56
Descriptive Properties Value Comments
Aniline Point 163°F
Method E, ASTM D611
Aromatic Content 0.29
GC, ExxonMobil Method
Dry Point 606°F
ASTM D86
Copyright © lookpolymers.com All Rights Reserved