CAS Number: 68526-58-9Appearance: Clear, free of suspended matterInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.768 - 0.774 g/cc
0.0277 - 0.0280 lb/in³
ECIM-1009
Descriptive Properties Value Comments
Color <10
Platinum Cobalt, ECIM-1003
Composition < C9
<0.75%, ECIM-2012
>C14
<0.7%, ECIM-2012
C10
4-6%, ECIM-2012
C11
18-21.5%, ECIM-2012
C12
69.5-77%, ECIM-2012
C13
<3.5%, ECIM-2012
Peroxides, active oxygen
<5 ppm, ECIM-3006
Sulfur
<10 ppm, ECIM-2004
Water
<100 ppm, ECIM-3003