ExxonMobil Santoprene® 8211-85M350 Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8211-85M350 Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is developed to be used as a skin for molding onto rigid polypropylene substrates on automotive interior applications such as door panels and center consoles. For these applications, this grade combines low gloss, high scratch and mar resistance, low emissions (fogging, odor) and "comfort touch". This grade of Santoprene TPV is shear-dependent and can be processed on conventional mono- and multi-component injection molding machines. It is polyolefin based, adheres to and is compatible with polypropylene, and is completely recyclable.Key Features:Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Designed for applications requiring high-flow materials.Cost effective alternative to soft touch paint over PP substrate.EU and China RoHS compliant.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 86

@Time 15.0 sec
86

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 8.80 MPa
1280 psi
Across Flow; ASTM D412 and ISO 37
Elongation at Break 480 %
480 %
Across Flow; ASTM D412 and ISO 37