Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 201-55W255 Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 201-55W255 Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and contains a stabilization system for protection against copper and other metal-catalyzed degradation. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:EU and China RoHS compliant.Applications:Appliance- Seals and GasketsUses:Appliance ComponentsGasketsSealsProcessing Method: Coextrusion, Injection Molding, Profile Extrusion, Extrusion, Multi Injection Molding and Sheet Extrusion Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 15.0 sec
60

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 5.10 MPa
740 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 450 %
450 %
Across Flow; ASTM D412 and ISO 37
Compression Set 16 %

@Temperature 23.0 °C,
Time 79200 sec
16 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
42 %

@Temperature 100 °C,
Time 79200 sec
42 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
47 %

@Temperature 100 °C,
Time 1.08e+6 sec
47 %

@Temperature 212 °F,
Time 300 hour
ASTM D395B Type 1 and ISO 188 Type A