ExxonMobil Santoprene® 151-60 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 151-60 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.Features: Excellent flex fatigue resistanceExcellent Ozone ResistanceProduct Notes: Values are for injection molded plaques, side gated.102 mm x 152 mm x 2 mmInformation provided by Advanced Elastomer Systems.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
5 seconds; ASTM D2240
Tensile Strength at Break 2.40 MPa
348 psi
Across flow; ASTM D412
Tensile Strength, Yield 1.20 MPa

@Strain 100 %
174 psi

@Strain 100 %
across flow; ASTM D412
Elongation at Break 350 %
350 %
Across flow; ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 26 %
26 %
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant Dryer
Dry Time 3 hour
3 hour
Desiccant Dryer