Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and contains a stabilization system for protection against copper and other metal-catalyzed degradation. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada -Component.EU and China RoHS compliant.Applications:Appliance - Dishwasher Seals and GasketsUses:Appliance ComponentsGasketsSeal Processing Method: Coextrusion, Injection Molding, Profile Extrusion, Extrusion, Multi Injection Molding and Sheet ExtrusionAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
0.078 in; ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
Across Flow; ASTM D412
Tensile Stress 1.40 MPa

@Strain 100 %
203 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 400 %
400 %
Across Flow; ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.70 mm
HB

@Thickness 0.0669 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 0.35
Color Black
Form Pellets
Copyright © lookpolymers.com All Rights Reserved