Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP5032E3 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP5032E3 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A polypropylene homopolymer type designed for production of monofilaments, tapes for the textile industry, geo textiles, fibrillated tapes for ropes and twines in the packaging, agriculture and finishing industries and suitable for chill roll and water bath lines.Availability: Africa & Middle East and Asia Pacific Features:Low Water Carryover Uses: Consumer ApplicationsFabricsFibers Heavy-duty BagsPackaging Processing Method: Extrusion, Filament Extrusion and ThermoformingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2/1A/50
Elongation at Yield 9.0 %
9.0 %
ISO 527-2/1A/50
Tensile Modulus 1.44 GPa
209 ksi
ISO527-2/1A/1
Flexural Modulus 1.43 GPa
207 ksi
0.079 in/min; ISO 178
Charpy Impact, Notched 0.441 J/cm²
2.10 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 320 °C
608 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
ISO 75-2/B