Material Notes:
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableEthylene Oxide SterilizableLow ExtractablesSteam SterilizableUses: LabwareMedical PackagingMedical/Healthcare ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868
Tensile Strength, Yield 33.0 MPa
4790 psi
ISO 527-2/50
Elongation at Yield 8.0 %
8.0 %
ISO 527-2/50
Tensile Modulus 1.50 GPa
218 ksi
ISO 527-2/1
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Izod Impact, Notched (ISO) 2.31 kJ/m²
1.10 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.399 J/cm²

@Temperature 22.8 °C
1.90 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 320 °C
608 °F
ISO 3149
Crystallization Temperature 235 °C
455 °F
ISO 3164
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ISO 75-2/A
Vicat Softening Point 153 °C
307 °F
ISO 306/A50