Material Notes:
Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machines, especially when laminated with PET. Due to the consistent slip properties, it can be also used in most VFFS applications. In addition to this, the improved barrier properties make it an excellent choice for sensitive product packaging, combining great product protection and yield advantage.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Broad sealing range on the inside filmGood hot tack and very good seal integrityVery good moisture and light barrierGood oxygen barrierExcellent adhesion of aluminum to filmEasy to convertOutstanding metal appearanceConsistent slip propertiesFeatures: Flavor & Aroma BarrierGas BarrierIn Lamination Lap SealableLight BarrierMoisture BarrierOxygen Barrier Applications:BakeryBiscuits/Cookie/CrackersConfectionery, Chocolate Confectionery, Gum Confectionery, Sugar Crisps and SnacksFrozen FoodHousehold and DetergentsIce Cream Pet Food Uses:Box Overwrap Flexible Packaging HFFS Flexible Packaging Pre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Solvent Flexographic Printing and Solvent Rotogravure PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 2.95 g/m²/day

@Temperature 38.0 °C
0.190 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 49.7 cc/m²/day

@Temperature 23.0 °C
3.20 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
50.1 cc/m²/day

@Temperature 23.0 °C
3.23 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
Thickness 15.0 microns
0.590 mil
ExxonMobil Method
Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 205 %
205 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 55 %
55 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 2.00 GPa
290 ksi
MD; ExxonMobil Method
3.70 GPa
537 ksi
TD; ExxonMobil Method
Coefficient of Friction 0.50
0.50
VBSR; ExxonMobil Method
Seal Strength 460 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
460 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
Film Tensile Strength at Break, MD 140 MPa
20300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 290 MPa
42100 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %

@Temperature 135 °C,
Time 432 sec
4.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 4.0 %

@Temperature 135 °C,
Time 432 sec
4.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Optical Density 2.3
2.3
ExxonMobil Method
Descriptive Properties Value Comments
Heat Seal Range 99°F
36.3 psi, 0.2 sec
Yield 51500 in2/lb